@ -214,4 +214,19 @@ TPE enhanced with the same chemicals used to make ABS.
- Horrible to print in every way
- Useful for purging the nozzle when switching between high and low temp filaments
# POM (Polyoxylmetn)
# POM (Polyoxylmethylene)
POM is most commonly used when CNCing plastic.
- It's cheap and very easy to print, with a low coefficient of friction.
- Zero bed adhesion
- Very poor layer adhesion
- When it overheats, it turns into formaldehyde
# PVDF (Polyvinylidene Flouride)
- A chemical cousin of teflon
- As easy to print as PET-G
- Extremely tough
- High heat/friction resistance
- Hydrophobic
- Most important because of its chemical resistance.
- Fairly expensive
- When mildly overheated, turns into horribly toxic chemicals (carbon monoxide, )