TL;dr:
- Use gyroid infill with an infill density of between 50-80% for structural prints
- Use PLA with a very slow speed, low layer height, and minimal/no cooling
- Use dovetail joints of scale defined in the HP article
- Anneal the print at 110c for ~30 minutes depending on the size and shape of the object